Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.77 J/cm²

@Temperature 23.0 °C
8.42 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 1.77 J/cm²
8.42 ft-lb/in²
Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Conditioned)
Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and ..
Charpy Impact, Notched 1.77 J/cm²
8.42 ft-lb/in²
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..