Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.300 - 55.0 J/cm² | 1.43 - 262 ft-lb/in² | Average value: 5.25 J/cm² Grade Count:29 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.500 - 55.0 J/cm² | 2.38 - 262 ft-lb/in² | Average value: 6.07 J/cm² Grade Count:10 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |