Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.20 - 11.5 J/cm² @Temperature -30.0 - -30.0 °C |
5.71 - 54.7 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.27 J/cm² Grade Count:6 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |