Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.980 - 1.02 J/cm²

@Temperature -30.0 - -30.0 °C
4.66 - 4.85 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.00 J/cm² Grade Count:2
Overview of materials for Nylon 11 with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are includ..
Charpy Impact, Notched 0.980 J/cm²

@Temperature -30.0 °C
4.66 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid..
Charpy Impact, Notched 0.980 J/cm²

@Temperature -30.0 °C
4.66 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig..