Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.980 - 1.02 J/cm²

@Temperature -30.0 - -30.0 °C
4.66 - 4.85 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.00 J/cm² Grade Count:2
Overview of materials for Nylon 11 with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are includ..