Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.884 J/cm² @Temperature 23.0 °C |
4.21 ft-lb/in² @Temperature 73.4 °F |
|
Micropol Microlin ML90 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |