Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Micropol Microlin ML90 Linear Polyethylene Rotational Molding Powder

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Manufacturer Micropol Limited
Trade Name Microlin
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Micropol Microlin ML90 Linear Polyethylene Rotational Molding Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Micropol Limited
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
ASTM D792
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
10.4 g/10 min

@Load 5.00 kg,
Temperature 190 °C
10.4 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
50mm/min; ASTM D638-64T
Elongation at Break 239 %
239 %
ASTM D638-64T
Modulus of Elasticity 0.685 GPa
99.4 ksi
ASTM D638
Charpy Impact, Notched 0.884 J/cm²

@Temperature 23.0 °C
4.21 ft-lb/in²

@Temperature 73.4 °F
Impact 16.4

@Temperature -20.0 °C
16.4

@Temperature -4.00 °F
J/mm, Falling weight impact; ARM
Thermal Properties Metric English Comments
Vicat Softening Point 117 °C
243 °F
ASTM D1525
Copyright © lookpolymers.com All Rights Reserved