Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.884 J/cm²

@Temperature 23.0 °C
4.21 ft-lb/in²

@Temperature 73.4 °F
Micropol Microlin ML90 Linear Polyethylene Rotational Molding Powder
Information provided by Micropol Limited