Polymer Property : Charpy Impact, Notched = 3.66 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.770 J/cm²

@Temperature -30.0 °C
3.66 ft-lb/in²

@Temperature -22.0 °F
Eastman Eastalloy DA003 PC+PCTG Copolyester/Polycarbonate  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 0.770 J/cm²
3.66 ft-lb/in²
ISO 179/1eA
NOVA Chemicals Dylark® 378P12 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
Charpy Impact, Notched 0.770 - 1.38 J/cm²
3.66 - 6.57 ft-lb/in²
Average value: 1.05 J/cm² Grade Count:5
Overview of materials for Glass Reinforced, Modified SMA
This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.770 J/cm²

@Temperature -30.0 °C
3.66 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS Lustran® 648
Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding
Charpy Impact, Notched 0.770 J/cm²
3.66 ft-lb/in²
ISO 179/1eA
Polyplastics FR-PET® B3045FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
Charpy Impact, Notched 0.770 J/cm²
3.66 ft-lb/in²
ISO 179/1eA
DuPont Performance Polymers Crastin® CE15330 BK010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V..
Charpy Impact, Notched 0.770 J/cm²

@Temperature -30.0 °C
3.66 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AESN TL Nylon 12, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA12,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. Good chemical resistance. Very good ability ..