Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.770 J/cm² @Temperature -30.0 °C |
3.66 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastalloy DA003 PC+PCTG Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.770 J/cm² | 3.66 ft-lb/in² | ISO 179/1eA |
NOVA Chemicals Dylark® 378P12 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Charpy Impact, Notched | 0.770 - 1.38 J/cm² | 3.66 - 6.57 ft-lb/in² | Average value: 1.05 J/cm² Grade Count:5 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.770 J/cm² @Temperature -30.0 °C |
3.66 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® 648 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 0.770 J/cm² | 3.66 ft-lb/in² | ISO 179/1eA |
Polyplastics FR-PET® B3045FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Charpy Impact, Notched | 0.770 J/cm² | 3.66 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® CE15330 BK010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V.. |
|||
Charpy Impact, Notched | 0.770 J/cm² @Temperature -30.0 °C |
3.66 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AESN TL Nylon 12, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA12,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. Good chemical resistance. Very good ability .. |