Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.510 J/cm²
2.43 ft-lb/in²
ASTM D256
Plenco 6990 Phenolic, Briquette, Compression Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Charpy Impact, Notched 0.510 J/cm²
2.43 ft-lb/in²
ISO 179/1eA
Polyplastics Tepcon M320 Acetal-copolymer (POM), High Fluidity, High Cycle
Information provided by PolyPlastics.
Charpy Impact, Notched 0.510 J/cm²
2.43 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 3116 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 7.5% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.510 J/cm²
2.43 ft-lb/in²
ISO 179/1eA
DuPont Performance Polymers Crastin® CE15315 BK010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0..
Charpy Impact, Notched 0.510 J/cm²

@Temperature 23.0 °C
2.43 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Charpy Impact, Notched 0.510 J/cm²
2.43 ft-lb/in²
1eA; ISO 179
Azoty Tarnow™ TARNOFORM 500 GF6 POM
30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr..
Charpy Impact, Notched 0.510 J/cm²
2.43 ft-lb/in²
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Conditioned)
Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp..