Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI)

Category Polymer , Thermoplastic , Polyimide, Thermoplastic , Thermoplastic Polyimide, Glass Fiber
Manufacturer Ensinger
Trade Name TECASINT
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.Main FeaturesHigh thermal and mechanical capacityHigh gamma radiation resistanceGood chemical resistanceEasily machinedFlame retardant according to UL94 V-0Very creep resistantGood wear propertiesLow coefficient of thermal expansionVery good electrical insulationSensitive to hydrolysis in higher thermal rangeApplicationsMechanical engineeringCryogenicsAircraft and aerospace industriesElectronicsNuclear and vacuum technologyElectrical engineeringPreferred FieldsSwitch parts, connector, housing, lead backerInformation Provided by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.57 g/cc

@Temperature 23.0 °C
0.0567 lb/in³

@Temperature 73.4 °F
DIN 53 479
Filler Content 30 %
30 %
Glass Fiber
Water Absorption 3.13 %

@Temperature 80.0 °C
3.13 %

@Temperature 176 °F
3 week saturation; EN ISO 62
0.53 %

@Temperature 23.0 °C,
Time 86400 sec
0.53 %

@Temperature 73.4 °F,
Time 24.0 hour
EN ISO 62
1.66 %

@Temperature 80.0 °C,
Time 86400 sec
1.66 %

@Temperature 176 °F,
Time 24.0 hour
EN ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 92

@Temperature 23.0 °C
92

@Temperature 73.4 °F
DIN 53 505
Tensile Strength, Yield 94.0 MPa

@Temperature 23.0 °C
13600 psi

@Temperature 73.4 °F
EN ISO 527
Elongation at Break 3.4 %

@Temperature 23.0 °C
3.4 %

@Temperature 73.4 °F
EN ISO 527
Elongation at Yield 3.1 %
3.1 %
Flexural; EN ISO 178
Tensile Modulus 5.80 GPa

@Temperature 23.0 °C
841 ksi

@Temperature 73.4 °F
EN ISO 527
Flexural Strength 163 MPa

@Temperature 23.0 °C
23600 psi

@Temperature 73.4 °F
EN ISO 178
Flexural Modulus 6.625 GPa

@Temperature 23.0 °C
960.9 ksi

@Temperature 73.4 °F
EN ISO 178
Compressive Strength 260 MPa

@Temperature 23.0 °C
37700 psi

@Temperature 73.4 °F
EN ISO 604
Charpy Impact Unnotched 2.73 J/cm²
13.0 ft-lb/in²
EN ISO 179
Charpy Impact, Notched 0.510 J/cm²

@Temperature 23.0 °C
2.43 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Compression Set 72 %
72 %
Compression at Break; EN ISO 604
Thermal Properties Metric English Comments
CTE, linear 33.0 µm/m-°C

@Temperature 50.0 - 200 °C
18.3 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Glass Transition Temp, Tg 340 °C
644 °F
DMTA
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+14 ohm

@Temperature 23.0 °C
>= 1.00e+14 ohm

@Temperature 73.4 °F
IEC 60093
Dielectric Constant 3.59

@Frequency 1000 Hz,
Temperature 23.0 °C
3.59

@Frequency 1000 Hz,
Temperature 73.4 °F
IEC 60250
Descriptive Properties Value Comments
Color Dark Brown
DIN-Abbreviation PAI GF30