Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.530 MPa @Strain 40.0 % |
76.9 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® HD80 High Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Compressive Yield Strength | 0.530 MPa @Strain 50.0 % |
76.9 psi @Strain 50.0 % |
ASTM 1056/85 |
Eurofoam Gummicell GU 250 0,70 NR Foam Natural rubber foam. Uses: industrial purposes, ceramics, mouse pads, diecutting, eletronics, and electromechanicsInformation provided by Eurofoam s.r.l. |