Natural rubber foam. Uses: industrial purposes, ceramics, mouse pads, diecutting, eletronics, and electromechanicsInformation provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.630 - 0.770 g/cc
0.0228 - 0.0278 lb/in³
ISO 845-88
Water Absorption <= 3.5 %
<= 3.5 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 65 - 75
65 - 75
ASTM D 2240
Tensile Strength 0.400 MPa
58.0 psi
ASTM D 412
Elongation at Break >= 500 %
>= 500 %
ASTM D 412
Compressive Yield Strength 0.260 MPa

@Strain 25.0 %
37.7 psi

@Strain 25.0 %
ASTM 1056/85
0.530 MPa

@Strain 50.0 %
76.9 psi

@Strain 50.0 %
ASTM 1056/85
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
ASTM D 3575
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
ASTM D 3575
Descriptive Properties Value Comments
Cellular Structure Closed
Color Green
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC