Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 111 MPa
16100 psi
ISO 2039-1
Covestro Makrolon® 3100 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Ball Indentation Hardness 111 - 118 MPa
16100 - 17100 psi
Average value: 115 MPa Grade Count:35
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..