Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 111 MPa | 16100 psi | ISO 2039-1 |
Covestro Makrolon® 3100 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Ball Indentation Hardness | 111 - 118 MPa | 16100 - 17100 psi | Average value: 115 MPa Grade Count:35 |