Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 111 - 118 MPa | 16100 - 17100 psi | Average value: 115 MPa Grade Count:35 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |