Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 13.6 J @Treatment Temp. 496 °C |
10.0 ft-lb @Treatment Temp. 925 °F |
hardened H925; V-notch |
Crucible Steel CSM® 21 17Cr-4Ni Precipitation Hardening Stainless Steel CSM 21 is a precipitation hardening stainless mold steel, providing outstanding corrosion resistance and toughness, good polishability, and moderate wear resistance, combined with simple heat treatm.. |
|||
Charpy Impact | 13.6 J @Tempering Temp. 566 °C |
10.0 ft-lb @Tempering Temp. 1050 °F |
air cooled from 1900°F then tempered; V-notch |
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |