Mechanical Properties Metric English Comments
Charpy Impact 13.6 J

@Treatment Temp. 496 °C
10.0 ft-lb

@Treatment Temp. 925 °F
hardened H925; V-notch
Crucible Steel CSM® 21 17Cr-4Ni Precipitation Hardening Stainless Steel
CSM 21 is a precipitation hardening stainless mold steel, providing outstanding corrosion resistance and toughness, good polishability, and moderate wear resistance, combined with simple heat treatm..
Charpy Impact 13.6 J

@Tempering Temp. 566 °C
10.0 ft-lb

@Tempering Temp. 1050 °F
air cooled from 1900°F then tempered; V-notch
Crucible Steel WR-95 Tool Steel, AISI H10 Modified
WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight..