Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 36.2 - 38.0 J | 26.7 - 28.0 ft-lb | Average value: 36.5 J Grade Count:5 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |