Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D5420 |
RheTech Products FT4700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Network Polymers Softflex® 0150 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP2-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Gardner Impact | 36.2 - 36.2 J | 26.7 - 26.7 ft-lb | Average value: 36.2 J Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC/TP-GP1 PC Polyester, High Impact, Good Chemical Resistance
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources NY6-IM1-[color]-H Nylon 6, Impact Modified, Heat Stabilized Nylon 6, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Gardner Impact | 36.2 J @Temperature -30.0 °C |
26.7 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
DuPont Bexloy® AXW507NC010 Modified Ionomer Resin
(discontinued **) A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Gardner Impact | 36.2 J @Temperature -30.0 °C |
26.7 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
DuPont Bexloy® AXW504BK Modified Ionomer Resin
(discontinued **) A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Gardner Impact | 36.2 J @Temperature -30.0 °C |
26.7 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
DuPont Bexloy® AXW602NC010 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin
(discontinued **) A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | ASTM D5420 |
Flint Hills P5C4K-089 Random Copolymer Polypropylene Features: Good clarity. Product does not contain animal derived components. Phthalate-freeApplications: Cast FilmInformation provided by Flint Hills Resources. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D5420 |
Flint Hills P5M6K-101X Random Copolymer Polypropylene Features: Excellent clarity and processing. Product does not contain animal derived components. Phthalate-freeApplications: Injection molding - high clarity parts and medical devicesInformation .. |
|||
Gardner Impact | 36.2 J @Thickness 3.17 mm, Temperature 23.0 °C |
26.7 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D5420, GB |
Ineos Styrenics Avantra® 594E High Impact Styrenic Polymer (NAFTA) Description: Avantra® 594E is a super high-impact polystyrene grade that delivers excellent processing efficiency along with toughness and high gloss in a wide variety of injection molding applic.. |
|||
Gardner Impact | 36.2 J @Temperature 23.0 °C |
26.7 ft-lb @Temperature 73.4 °F |
ASTM D 5420 |
Shakespeare Isocorâ„¢ HG26SI medium viscosity PA-612 Isocorâ„¢ HG26SI is a medium viscosity PA-612 based nylon. This resin is specifically suited for applications requiring low moisture regain and greater dimensional stability. Isocorâ„¢ HG2.. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Diamond Polymers NPP 60-3301 Clear Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | CP-TM-11 |
PolyOne Elastamax HTE 2101-1002 Polyurethane Alloy
(discontinued **) This is an extrusion grade polyurethane alloy. Physical Form: Pellet. Standard Color: Off white, opaque.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. .. |