Mechanical Properties Metric English Comments
Gardner Impact 34.0 J
25.1 ft-lb
No Break
Plaskolite PETG Mirror Sheet
Versatile fabrication properties with good impact strength, good design flexibility, and speed of fabrication.Data provided by the manufacturer, Plaskolite, Inc.
Gardner Impact 34.0 - 36.0 J

@Temperature -30.0 - -30.0 °C
25.1 - 26.6 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 36.2 J Grade Count:6
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m..
Gardner Impact 34.0 - 36.0 J
25.1 - 26.6 ft-lb
Average value: 34.5 J Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is ..
Gardner Impact 34.0 J

@Temperature 23.0 °C
25.1 ft-lb

@Temperature 73.4 °F
ASTM D5420
Flint Hills AP5995-HA Polypropylene Impact Copolymer
Features: Nucleated with slip, fast cycle times, high flowability.Applications: Injection Molding: High speed packaging applications and thin wall containersInformation Provided by Flint Hills Resou..
Gardner Impact 34.0 J

@Temperature -30.0 °C
25.1 ft-lb

@Temperature -22.0 °F
ASTM D3029
LyondellBasell Hifaxâ„¢ ETA-3081 Thermoplastic Olefin Resin
Key Features: medium high melt flow, medium modulus, paintable thermoplastic olefin resin, excellent balance of properties, excellent processability, good paintability and paint durability, good sur..
Gardner Impact 34.0 J

@Temperature -30.0 °C
25.1 ft-lb

@Temperature -22.0 °F
ASTM D3029, tested in accordance with ASTM D5420
LyondellBasell Hifaxâ„¢ ETA3081HS Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ ETA3081HS medium melt flow, 800 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has balanced physical properties, moldability and paintability. ..
Gardner Impact 34.0 J

@Temperature 23.0 °C
25.1 ft-lb

@Temperature 73.4 °F
SABIC Method
SABIC Innovative Plastics Ultem 1010RF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg..