Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 21.5 J @Temperature -30.0 °C |
15.8 ft-lb @Temperature -22.0 °F |
Method G, geometry GC; ASTM D5420 |
Pinnacle Polymers 3220 Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Gardner Impact | 21.5 J @Thickness 3.18 mm, Temperature 23.0 °C |
15.9 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D3029 |
PolyOne Maxxam™ FR PE 161 HDPE
(discontinued **) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Gardner Impact | 21.5 J @Thickness 3.17 mm, Temperature -28.9 °C |
15.8 ft-lb @Thickness 0.125 in, Temperature -20.0 °F |
Geometry GC; ASTM D5420 |
ExxonMobil AXO3BE3 Polypropylene Homopolymer Product Description: A high crystallinity, medium impact copolymer resin designed for injection-molded automotive interior applications and large appliance parts applications requiring high melt fl.. |