Polymer Property : Gardner Impact = 19.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 12.4 - 19.0 J
9.15 - 14.0 ft-lb
Average value: 15.8 J Grade Count:4
Overview of materials for Polypropylene w/ 50% Calcium Carbonate
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene w/ 50% Calcium Carbonate". Specific grades with calcium carbonate content between 45% and ..