Mechanical Properties Metric English Comments
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D5420
RheTech Products F43-01B 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Drip trayFunctional supportsA/C housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D5420
RheTech Products F49-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Fan shroudsSupport ductsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D5420
RheTech Products GC30P100-01UV 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black
Applications: Exterior automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D5420
RheTech Products M25UVP250-01 25% Mica Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: BracketsCowl screensRigid exterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D5420
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black
Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D5420
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D5420
RheTech Products F35-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Interior trimUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D5420
RheTech Products G30P100-00 30% Glass Fiber Reinforced Polypropylene, Natural
Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 0.565 - 21.7 J
0.417 - 16.0 ft-lb
Average value: 4.47 J Grade Count:22
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D3029
Plastics Group Polifil® T-40 40% Talc-Reinforced Polypropylene
Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora..
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D3029
Plastics Group Polifil® T-10 10% Talc-Reinforced Polypropylene
Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora..
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D3029
Plastics Group Polifil® T-20 20% Talc-Reinforced Polypropylene
Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora..
Gardner Impact 0.565 J
0.417 ft-lb
ASTM D3029
Plastics Group Polifil® T-30 30% Talc-Reinforced Polypropylene
Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora..
Gardner Impact 0.565 - 33.9 J
0.417 - 25.0 ft-lb
Average value: 5.46 J Grade Count:32
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
Gardner Impact 0.565 - 13.6 J
0.417 - 10.0 ft-lb
Average value: 2.05 J Grade Count:32