Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 1.47 - 33.9 J | 1.08 - 25.0 ft-lb | Average value: 14.6 J Grade Count:21 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Gardner Impact | 0.565 - 33.9 J | 0.417 - 25.0 ft-lb | Average value: 5.46 J Grade Count:32 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |