Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 0.500 J | 0.369 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 2005 M 20% Mica Filled Polypropylene Multi-Pro 2005 M is a mica reinforced polypropylene compound with high stiffness and flex strength. Its high heat resistance lends itself to replace engineered plastics at moderate cost.Data provid.. |
|||
Gardner Impact | 0.500 J | 0.369 ft-lb | reported as J/cm; ASTM D3029-GB, unpainted |
Plaskolite Optix® SG Sign Grade Acrylic Sheet Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Gardner Impact | 0.500 J @Temperature 23.0 °C |
0.369 ft-lb @Temperature 73.4 °F |
|
Diamond Polymers NPP30-0800 GF40 40% Glass Filled Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | 0.500 J @Temperature 23.0 °C |
0.369 ft-lb @Temperature 73.4 °F |
|
Diamond Polymers NPP30-2000 GF30 30% Glass Filled Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | 0.500 J | 0.369 ft-lb | ASTM D3029 |
Adell EL-16 Homopolymer Polypropylene, 30% Mineral Filled; Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Gardner Impact | 0.500 J | 0.369 ft-lb | ASTM D3029 |
Adell EQ-16 Homopolymer Polypropylene, 30% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Gardner Impact | 0.500 J | 0.369 ft-lb | ASTM D3029 |
Adell ER-14 Homopolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Gardner Impact | 0.500 J | 0.369 ft-lb | ASTM D3029 |
Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Gardner Impact | 0.500 J | 0.369 ft-lb | ASTM D5420 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3230A PP SABIC® PPcompound G3230A is a general purpose, 30% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 109612410 |