Diamond Polymers NPP30-2000 GF30 30% Glass Filled Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP30-2000 GF30 30% Glass Filled Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.0 MPa
7110 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 3.0 %
3.0 %
chs 2.0 in/min; ASTM D638
Flexural Strength 72.0 MPa
10400 psi
ASTM D790
Flexural Modulus 4.272 GPa
619.6 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Gardner Impact 0.500 J

@Temperature 23.0 °C
0.369 ft-lb

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
309 °F
0.125";; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
289 °F
0.125";; ASTM D648
Descriptive Properties Value Comments
Glass Content (%) 30
ASTM D2584