Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 1160 kJ/m² @Temperature 23.0 °C |
550 ft-lb/in² @Temperature 73.4 °F |
ASTM D1822 |
DuPont™ Surlyn® 8528 Sodium Ionomer Surlyn® 8528 is a sodium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 8528 thermoplastic resi.. |