Tensile Impact Strength 1160 kJ/m²

@Temperature 23.0 °C
550 ft-lb/in²

@Temperature 73.4 °F
ASTM D1822
DuPont™ Surlyn® 8528 Sodium Ionomer
Surlyn® 8528 is a sodium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 8528 thermoplastic resi..