Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 44.5 J/cm @Temperature 23.0 °C |
0.0834 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion 87768 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Dart Drop Total Energy | 44.5 - 280 J/cm | 0.0834 - 0.525 ft-lb/mil | Average value: 119 J/cm Grade Count:22 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Dart Drop Total Energy | 44.5 J/cm | 0.0833 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F(23°C); ASTM D4226 |
PolyOne Elastamax® HTE 2101 Thermoplastic Elastomer - PVC/TPU
(discontinued **) Description/Features:InteriorUL 94 V0Applications:General PurposeCustom Profiles-ComplexProcessing Method:Extrusion-Single ScrewInformation provided by PolyOne Corporation. |