PolyOne Elastamax® HTE 2101 Thermoplastic Elastomer - PVC/TPU  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax® HTE 2101 Thermoplastic Elastomer - PVC/TPU  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:InteriorUL 94 V0Applications:General PurposeCustom Profiles-ComplexProcessing Method:Extrusion-Single ScrewInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Melt Flow 13.67 g/10 min

@Load 8.70 kg,
Temperature 190 °C
13.67 g/10 min

@Load 19.2 lb,
Temperature 374 °F
Procedure B - Automatic Timed; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
15 sec; ASTM D2240
Tensile Strength, Yield 24.8 MPa
3600 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Tensile Modulus 1.45 GPa
210 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 41.4 MPa
6000 psi
ASTM D790
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790
Izod Impact, Notched 10.1 J/cm

@Thickness 3.17 mm
19.0 ft-lb/in

@Thickness 0.125 in
Method A, Compression Molded; ASTM D256
Dart Drop Total Energy 44.5 J/cm
0.0833 ft-lb/mil
Procedure A, 0.125 in Conical Dart, 73°F(23°C); ASTM D4226
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 57.2 °C
135 °F
Annealed; ASTM D648
Flammability, UL94 V-0
V-0
Natural, 0.062 in thick; UL 94