Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 44.5 - 280 J/cm | 0.0834 - 0.525 ft-lb/mil | Average value: 119 J/cm Grade Count:22 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Dart Drop Total Energy | 5.34 - 280 J/cm | 0.0100 - 0.525 ft-lb/mil | Average value: 91.9 J/cm Grade Count:160 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |