Polymer Property : Dart Drop Total Energy = 5.34 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Total Energy 5.34 - 178 J/cm
0.0100 - 0.333 ft-lb/mil
Average value: 70.9 J/cm Grade Count:38
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
Dart Drop Total Energy 5.34 - 280 J/cm
0.0100 - 0.525 ft-lb/mil
Average value: 91.9 J/cm Grade Count:160
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..