Polymer Property : 200% Modulus = 1.20 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.00827 GPa
1.20 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
200% Modulus 0.00827 GPa
1.20 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 310ºF Cure Temperature
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
200% Modulus 0.00827 GPa
1.20 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
200% Modulus 0.00827 GPa
1.20 ksi
ASTM D412
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane
Type: Estane® AG 8451 is a polyether based aliphatic (TPU) specifically formulated to be used as an adhesive interlayer film. AG-8451 is an excellent general purpose polymer for all optical allpha..
200% Modulus 0.00827 GPa
1.20 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
200% Modulus 0.00827 GPa
1.20 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
200% Modulus 0.00827 GPa
1.20 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 310ºF Cure Temperature
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..