Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00827 GPa | 1.20 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
200% Modulus | 0.00827 GPa | 1.20 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 310ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
200% Modulus | 0.00827 GPa | 1.20 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
200% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D412 |
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane Type: Estane® AG 8451 is a polyether based aliphatic (TPU) specifically formulated to be used as an adhesive interlayer film. AG-8451 is an excellent general purpose polymer for all optical allpha.. |
|||
200% Modulus | 0.00827 GPa | 1.20 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00827 GPa | 1.20 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00827 GPa | 1.20 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 310ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |