Polymer Property : 200% Modulus = 0.624 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.00430 GPa
0.624 ksi
ASTM D412
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.