Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00430 GPa | 0.624 ksi | ASTM D412 |
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |