Mechanical Properties Metric English Comments
Izod Impact Resistance 1.60 J/cm²
7.61 ft-lb/in²
ISO 180
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50
Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and..
Izod Impact Resistance 1.60 J/cm²
7.61 ft-lb/in²
ISO 180
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50
Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope..
Izod Impact Resistance 1.60 J/cm²
7.61 ft-lb/in²
Dow DOWLEX™ IP-60 High Density Polyethylene