Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 180 |
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50 Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and.. |
|||
Izod Impact Resistance | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 180 |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Izod Impact Resistance | 1.60 J/cm² | 7.61 ft-lb/in² | |
Dow DOWLEX™ IP-60 High Density Polyethylene DOWLEX® IP-60 resin is an improved processing high density polyethylene resin designed to offer excellent processability, good impact and top load strength required in thin wall injection molding. .. |