Dow DOWLEX™ IP-60 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Dow Chemical
Trade Name DOWLEX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow DOWLEX™ IP-60 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOWLEX® IP-60 resin is an improved processing high density polyethylene resin designed to offer excellent processability, good impact and top load strength required in thin wall injection molding. This resin is designed by optimization of the breadth, shape of the molecular weight distribution and peak molecular weight. It has demonstrated excellent processability over a wide range of molding conditions and in high cavitation molds. Typical applications are thin wall and food containers, promo drink cups, etc. It complies with FDA regulation 21 CFR 177.1520 (c) 3.1 for food contact applications.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
Melt Flow 60 g/10 min

@Load 2.16 kg
60 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.5.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.0 MPa
1450 psi
Tensile Strength, Yield 21.0 MPa
3050 psi
Elongation at Break 225 %
225 %
Modulus of Elasticity 0.641 GPa
93.0 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 0.869 GPa
126 ksi
Izod Impact Resistance 1.60 J/cm²
7.61 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 122 °C
252 °F