Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 180 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Izod Impact Resistance | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 180 |
Solvay Technyl® C 206 Nylon 6, EH50 Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f.. |
|||
Izod Impact Resistance | 8.01 J/cm² | 38.1 ft-lb/in² | |
Dow HDPE 17450N High Density Polyethylene DOW HDPE 17450N resin is a narrow molecular weight distribution copolymer designed to offer low temperature impact strength and gloss with excellent toughness. This resin has good processability ove.. |