Material Notes:
Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable for the production of technical molding with fast injection cycles. This product is available in natural.Information provided by Rhodia; Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183-A
Water Absorption 1.3 %
1.3 %
(Beginning Dry) 24 hours in water 23°C. ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Elongation at Break 270 %
270 %
ISO 527
Tensile Modulus 1.10 GPa
160 ksi
ISO 527
Flexural Yield Strength 40.0 MPa
5800 psi
ISO 178
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
Izod Impact Resistance 8.00 J/cm²
38.1 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 3146-C
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 93
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 93
Dielectric Constant 3.9

@Frequency 1e+6 Hz
3.9

@Frequency 1e+6 Hz
IEC 250
Dielectric Strength 18.0 kV/mm
457 kV/in
IEC 243-1
Dissipation Factor 0.10

@Frequency 1e+6 Hz
0.10

@Frequency 1e+6 Hz
IEC 250
Processing Properties Metric English Comments
Rear Barrel Temperature 220 - 230 °C
428 - 446 °F
Middle Barrel Temperature 225 - 235 °C
437 - 455 °F
Front Barrel Temperature 230 - 240 °C
446 - 464 °F