Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow HDPE 17450N High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow HDPE 17450N High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW HDPE 17450N resin is a narrow molecular weight distribution copolymer designed to offer low temperature impact strength and gloss with excellent toughness. This resin has good processability over a wide range of molding conditions. Typical applications are toys and housewares. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
Viscosity 75000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
75000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
140000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
140000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
200000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
200000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 17 g/10 min

@Load 2.16 kg
17 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.1 MPa
1900 psi
Tensile Strength, Yield 18.6 MPa
2700 psi
Elongation at Break 660 %
660 %
Modulus of Elasticity 0.593 GPa
86.0 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 0.862 GPa
125 ksi
Izod Impact Resistance 8.01 J/cm²
38.1 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C
253 °F