Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 44.0 J @Temperature -40.0 °C |
32.5 ft-lb @Temperature -40.0 °F |
At Max load; ASTM D3763 |
Eastman Aspira EN177 Copolyester Resin for Extrusion Blow Molding Applications:Beverage packagingConsumer packagingFood packagingPersonal care packagingKey Attributes:BPA-freeCompatible with high-output manufacturing platformsExcellent clarityHigh gloss appearance.. |
|||
Puncture Energy | 44.0 J @Thickness 3.20 mm, Temperature 23.0 °C |
32.5 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
max load; ISO 6603-2 |
Eastman Drystar 0601 Copolyester, Injection Molded This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Puncture Energy | 44.0 J @Temperature -40.0 °C |
32.5 ft-lb @Temperature -40.0 °F |
At Max load; ASTM D3763 |
Eastman Eastar GN119 Copolyester Applications:Personal care and CosmeticsProduct Description: Eastar GN119 Copolyester is a low-I.V. PETG, for sale only in Asia as a high-flow formulation. This product has been GREENGUARD INDOOR .. |
|||
Puncture Energy | 44.0 J @Temperature -40.0 °C |
32.5 ft-lb @Temperature -40.0 °F |
At Max load; ASTM D3763 |
Eastman Eastar GN120 Copolyester Applications:AppliancesConsumer electronicsPersonal care and cosmeticsStationary suppliesKey Attributes:High clarity and transparencyHigh flow copolyesterToughProduct Description: Eastar GN120 Cop.. |