Eastman Eastar GN119 Copolyester

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Eastar
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastar GN119 Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Personal care and CosmeticsProduct Description: Eastar GN119 Copolyester is a low-I.V. PETG, for sale only in Asia as a high-flow formulation. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.Information provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength at Break 24.0 MPa
3480 psi
ASTM D638
Tensile Strength, Yield 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 0.460 J/cm

@Temperature -40.0 °C
0.862 ft-lb/in

@Temperature -40.0 °F
ASTM D256
0.840 J/cm

@Temperature 23.0 °C
1.57 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Puncture Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
At Max load; ASTM D3763
44.0 J

@Temperature -40.0 °C
32.5 ft-lb

@Temperature -40.0 °F
At Max load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C
154 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Optical Properties Metric English Comments
Haze 0.40 %
0.40 %
ASTM D1003
Transmission, Visible 91 %
91 %
Total; ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 249 - 271 °C
480 - 520 °F
Mold Temperature 16.0 - 38.0 °C
60.8 - 100 °F
Drying Temperature 71.0 °C
160 °F
Dry Time 6 hour
6 hour