Polymer Property : Puncture Energy = 36.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 36.0 J

@Temperature 0.000 °C
26.6 ft-lb

@Temperature 32.0 °F
ISO 6603-2
Borealis BC545MO Polypropylene Copolymer
BC545MO is a low-blush polypropylene heterophasic copolymer intended for injection molding. This grade features high impact strength, high thermal stability and very good process ability. As all pol..
Puncture Energy 36.0 J

@Thickness 3.20 mm,
Temperature -40.0 °C
26.6 ft-lb

@Thickness 0.126 in,
Temperature -40.0 °F
max load; ISO 6603-2
Eastman Drystar 0601 Copolyester, Injection Molded
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..