Borealis BC545MO Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BC545MO Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC545MO is a low-blush polypropylene heterophasic copolymer intended for injection molding. This grade features high impact strength, high thermal stability and very good process ability. As all polypropylenes, this grade shows excellent stress-cracking and chemical resistances. This grade is characterized by combination of high stiffness, very high impact strength and low stress whitening. This grade is mildly nucleated to maximize the stiffness-impact balance. The additive formulation provides long-term heat stability. Its very good organoleptic properties allows this grade to be used with any master batch without discoloring problems. Applications: suitcases, battery cases, crates and boxes, and technical parts.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.908 g/cc
0.0328 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ISO 2039-2
Tensile Strength, Yield 25.0 MPa
3630 psi
50mm/min; ISO 527-2
Elongation at Yield 8.0 %
8.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.25 GPa
181 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Puncture Energy 36.0 J

@Temperature 0.000 °C
26.6 ft-lb

@Temperature 32.0 °F
ISO 6603-2
40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
196 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 230 - 260 °C
446 - 500 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity highest possible