Mechanical Properties Metric English Comments
Secant Modulus 9.98 GPa

@Strain 0.700 %,
Temperature 23.0 °C
1450 ksi

@Strain 0.700 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol..
Secant Modulus 9.98 GPa

@Strain 0.700 %,
Temperature 23.0 °C
1450 ksi

@Strain 0.700 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo..
Secant Modulus 9.98 GPa

@Strain 1.57 %,
Temperature -40.0 °C
1450 ksi

@Strain 1.57 %,
Temperature -40.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex..