Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 5.59 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 5.59 GPa

@Strain 1.04 %,
Temperature 0.000 °C
810 ksi

@Strain 1.04 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Secant Modulus 5.59 GPa

@Strain 1.68 %,
Temperature 0.000 °C
811 ksi

@Strain 1.68 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de..
Secant Modulus 5.59 GPa

@Strain 1.44095 %,
Temperature 0.000 °C
810 ksi

@Strain 1.44095 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..
Copyright © lookpolymers.com All Rights Reserved